Appearance: White, thixotropic liquid. Isophthalic gel coat, Medium reactivity, Accelerated, Light stabilized. Application: Sanitary, marine, etc.… Characteristics: Medium chemical resistance, Medium heat resistance, Resilient. Information provided by Polynt Composites. |