MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Röhm Plexiglas® 99845 Crystal Clear Elastomer Based Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA); Elastomer, TPE

Material Notes: Description: PLEXIGLAS® Clear Film 99845, based on polymethyl methacrylate and polybutyl acrylate elastomers, is absolutely crystal-clear. The film shows very good weather resistance and offers substrates excellent protection against natural UV radiation, of which it absorbs more than 98 %. Moreover, the film is resistant to stress whitening. The UV absorber is chemically bound and is not susceptible to migration.

Specific Notes for this Material: PLEXIGLAS® Film 99845 is suitable as a UV and weather protection film for colored or grained PVC window profiles and for protecting sheets and profiles made from PVC or glass-reinforced polyester. It offers UV protection for garden furniture with decorative surfacing as well as UV protection and upgrades surfaces for outside doors made of PVC or ABS.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors:
Available Properties
  • Density, ISO 1183
  • Film Tensile Strength at Yield, MD, ISO 527, no direction given
  • Film Elongation at Break, MD, ISO 527, no direction given
  • Film Elongation at Yield, MD, ISO 527, no direction given
  • Tensile Modulus, ISO 527
  • Volume Resistivity, IEC 250, No thickness given
  • Surface Resistance, IEC 250
  • Dissipation Factor, IEC 250
  • Dissipation Factor, IEC 250
  • CTE, linear, DIN 53752A
  • Specific Heat Capacity
  • Vicat Softening Point, ISO 306, Method B 50
  • Refractive Index, ISO 489
  • Haze, ASTM D1003
  • Yellow Index, ASTM D1925
  • Transmission, Visible, DIN 5036
  • UV Transmittance, DIN 5036
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.