MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Celanese Vamac® HVG Ethylene Methacrylate (AEM)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Vamac® HVG is an unfilled high viscosity gum ethylene/acrylic elastomer similar to Vamac® G, but offering higher compound viscosity. The higher viscosity of compounds made with Vamac® HVG results in improved green strength and related processing advantages, such as:
  • Improved collapse resistance of extrudates
  • Enhanced preform dimensional stability
  • Improved moldability through elimination of trapped air

Compounds of Vamac® HVG are often selected for applications such as compression molded goods, highly plasticized compounds, and extruded tubing and hose.

Vamac® HVG contains a small amount of processing aid.

Vamac® HVG is a Vamac® G type polymer with a Mooney Viscosity of 26 compared to 16 for Vamac® G. The two polymers have similar compositions but the Vamac® HVG has a higher molecular weight. They have many common features, including:

  • Good heat resistance in air
  • Good oil and fluid resistance
  • Good low temperature properties
  • Compounded with similar ingredients
  • Cured with same cure package

The big advantage of Vamac® HVG over Vamac® G is that the compounds made from the Vamac® HVG have a higher viscosity. The viscosity of the Vamac® HVG compound can be double that of a Vamac® G compound. This can lead to better processing. Specifically, the potential for a collapsed hose is reduced for an extrusion process and the potential for trapped air in an injection molded compound is reduced.

Former DuPont product acquired by Celanese in 2022.

Vendors:
Available Properties
  • Density, ISO 1183
  • Volatiles, EN 1400 / EN 14350-2
  • Mooney Viscosity, ISO 289-1-2, ML 1+4
  • Mooney Viscosity, ISO 289-1-2, ML 1+4, Compound
  • Hardness, Shore A, ASTM D 2240
  • Tensile Stress at Strain, ISO 527-1/-2
  • Compression Set, ISO 815
  • Maximum Service Temperature, Air, DuPont proprietary test
  • Processing Temperature
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Celanese (former DuPont Mobility and Materials)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.