Resulting from our purposeful selection of ultrapure initial raw materials and our deliberate engineered microstructure, parts manufactured from the newly developed aluminum oxide material provide: high corrosion resistance to chemical attacks ,high imperviousness in gaseous atmospheres, low creep tendency at high temperatures, high purity, high strength. Components show a strikingly high durability in the large variety of applications for sheath tubes.Information provided by Morgan Advanced Materials |