MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Radel® R-7700 Polyphenylsulfone (PPSU), Premium grade resin and deep draw sheet for thermoforming
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Premium grade resin and deep draw sheet for thermoforming, for aircraft interiors

Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, low smoke generation and low toxic gas emissions, thereby complying with the FAA regulation 14CFR Part 25.853 Appendix F. In addition, it has excellent impact resistance and meets typical industry requirements for resistance to aerospace fluids, even under stress.

Radel® R-7700 is available in pellets and sheet form.

Radel® R-7700 sheet can be formed into large complex geometries with relative ease on conventional thermoforming equipment. Please reference the Technical Bulletin Thermoforming Radel® R-7700 Sheet for additional information.

- Available in several custom colors

Markets/Uses: Aircraft / Aircraft Interiors / Extruded Profiles and Tubing; Aircraft / Aircraft Interiors / Flight Deck Components; Aircraft / Aircraft Interiors / Galley Carts and Boxes; Aircraft / Aircraft Interiors / Video Shrouds

Applications: Aerospace Applications; Aircraft Applications; Aircraft Interiors

Features: Detergent Resistant; Flame Retardant; Good Processing Stability; Good Toughness; Low Smoke Emission; Low Toxicity

The Federal Aviation Administration (FAA) has issued stringent regulations covering materials for use in commercial aircraft interiors. As shown in the Heat Release and Smoke Density data above, Radel R-7700 sheet complies with these regulations.

In addition, several airframe manufacturers have an additional requirement that, when these materials burn, any smoke generated contain no more than defined levels of specific toxic gases. Radel R-7700 polyphenylsulfone sheet typically exhibits levels of these gases that are much lower than the maximum levels allowed, see Toxic Gas Emission data above.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Gardner Impact, ASTM D3029
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.