MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LyondellBasell AlathonĀ® M4855 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 are consumer durables and 35, 65, and 95-gallon refuse carts.

Regulatory Status: Alathon M4855 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing M4855 can only be made when the processing conditions, equipment and end use application are known.

This product is from the former Equistar product line.

Vendors:
Available Properties
  • Bulk Density, ASTM D1895
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Spiral Flow, Equistar test
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Tensile Modulus, ASTM D638, 1% Secant; 50mm/min
  • Tensile Modulus, ASTM D638, 50mm/min
  • Flexural Modulus, ASTM D790, 12.5 mm/min
  • Flexural Modulus, ASTM D790, Secant; 12.5 mm/min
  • Flexural Modulus, 1% Secant, ASTM D790, 2.5 mm/min
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D4812
  • Melting Point, ASTM D3418
  • Crystallization Temperature, ASTM D3418
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.