MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Eastman Amphora™ FL6000 Flexible 3D Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Amphora™ Flex 3D polymer FL6000, a flexible material engineered for extrusion-based additive manufacturing processes. Amphora Flex FL6000 is a polymer that can be used with standard 3D printers, eliminating the need to switch to specialized flex extruders. Because of exceptional layer-to-layer adhesion and melt strength, it prints at a faster speed than other elastomeric materials, saving time. Amphora Flex FL6000 is an engineering-grade material that demonstrates superior durability and toughness, enabling designers to quickly create truly functional parts that can withstand the rigors of everyday use. Amphora Flex FL6000 is highly useful for applications that demand both the durability of an engineering-grade polymer and the comfort and utility of a flexible material. With a Shore A hardness level of 95, outstanding chemical resistance, and a temperature resistance that allows steam sterilization, users may find it useful for additive manufacturing of prosthetics, orthotics, automotive parts, apparel, tooling, or a variety of consumer products.

Application/Uses:

  • Production of 3D Printing filaments
Key Attributes:
  • Dimensional stability
  • Enhanced aesthetics
  • Excellent Temperature Resistance
  • Excellent toughness
  • Extended Processing Window
  • Low odor
  • Property retention in 3D applications
  • Steam Sterilizable
  • Styrene-free
  • Workability

Vendors:
Available Properties
  • Density, ASTM D792
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Tear Strength Test, ASTM D1004, N
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.