Temper: As Sand Cast Casting Characteristics: High – Fluidity; Medium – Shrinkage in Solidification, Casting Yield, Effect of Section Size, Gassing; Low –Drossing Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding Typical uses: Window Hardware; Bearings; Fittings; Gears; Impellers; Levers; Pump Fixtures; Valve Bodies; Boat Parts; Small Boat Propellers; Fixtures Applicable Specifications: As Centrifugal Cast - Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Permanent Mold Cast - Castings ASTM B806; As Sand Cast – Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30 |