MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dynasol SolpreneĀ® 4301 Thermoplastic Rubber (SBS)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Solprene 4301 is a linear block copolymer of styrene and butadiene, having 33% styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non-staining antioxidant system; FDA approved for use in food contact applications and is essentially gel free with a very clear color. It is presented as free flowing porous crumb making easy its handling and dissolution.

Uses: S-4301 is used as compounding ingredient for adhesives, as impact modifier for plastics and as elastomeric modifier for asphalt mixtures used in paving and roofing.

Applications:
Crack Sealant
Adhesives
Polymer modification
Paving
Roofing

Information provided by Dynasol.

Vendors:
Available Properties
  • Volatiles, ASTM D5668
  • Viscosity Measure, NM-300-11, 5.23% Toluene solution
  • Melt Flow, ASTM D1238
  • Styrene Content, NM 202-07, Block
  • Styrene Content, ASTM D5775
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.