The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gives the silicone fluids special usage properties. A surface covered with methyl silicone fluids reflects anti-adhesive properties, while the thin layer of oil remaining on it, is resistant to high temperature. Fluids may be sprayed both in the form of several-percent solution and non-diluted. In rubber processing also water emulsion of silicone fluids are used (Polsil® E), which are easy to dilute and apply.A surface covered with methyl silicone fluids reflects anti-adhesive properties, while the thin layer of oil remaining on it, is resistant to high temperature. Fluids may be sprayed both in the form of several-percent solution and non-diluted. In rubber processing also water emulsion of silicone fluids are used (Polsil® E), which are easy to dilute and apply. |