Unsaturated polyester resin in styrene, Isophthalic Appearance: NA Main resin characteristics: Low reactivity, Low exothermic peak, Preaccelerated, Thixotropic Main applications: General purpose, Marine, boats Molding information: Hand lay up and Spray up Curing cycle: 16 h at 40°C (+ 2 h at 120°C for HDT) Information provided by Polynt Composites. |