MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik Europlex® EC Transparent Plastic  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: EUROPLEX® EC is an impact-modified, transparent plastic with an electroconductive surface. This product is used wherever operational and workplace safety calls for glazing products that have to meet the following requirements:
  • antistatic or electroconductive surfaces (< 10E+6 ohm)
  • good transparency and light transmission
  • good impact resistance and dielectric strength
  • good abrasion resistance

EUROPLEX® EC is supplied in sheets of 1.0 to 8.0 mm thickness. In addition to clear sheets, a variety of application-specific colors are also available. The main fields of application are clean-room glazing, explosion-proofing and machine guards.

Information provided by degussa.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors:
Available Properties
  • Density, ISO 1183
  • Modulus of Elasticity, ISO 527-2/1B/1, short term value
  • Charpy Impact Unnotched, ISO 179/1fU
  • Abrasion, ISO 9352, % Haze, Abrasion resistance in Taber abrader test
  • Sound Insulation, Weighted Sound Reduction Index
  • Sound Insulation, Weighted Sound Reduction Index
  • Surface Resistivity per Square, DIN IEC 93 (VDE 0303/30)
  • CTE, linear, DIN 53752-A
  • Maximum Service Temperature, Air, Permanent
  • Flash Point, DIN 51794, Ignition Temperature
  • Transmission, Visible, DIN 5036, part 3, clear 99100
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.