BLACK PE-B1301 is a black low density polyethylene based masterbatch containing pure high opacity carbon black. It is designed for use in high jet black film with excellent surface performance, such as high opacity mulch. It also can provide premium tinting strength for Injection Molding items and Hollow Blown Films. Method of Usage: BLACK PE-B1301 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resin mixer, avoiding pollution and malscattering problems caused by pigment. Range of Application: BLACK PE-B1301 is designed for use in LDPE, HDPE, LLDPE and PP. |