MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Solvay VTS 243FR Epoxy Syntactic-Core Film
Categories: Polymer; Film; Thermoset; Epoxy

Material Notes: Description: VTS243FR is a black-pigmented, flame-retarded, epoxy syntactic-core film capable of initial cure temperatures between 65 and 150°C (149 and 30°F). Following post-cure, a Tg of at least 160°C(320°F) can be achieved. The material is formulated for co-cure with VTM®240 series of pregregs and VTF242FRB surfacing film. VTS243FR is self-extinguishing when tested to ISO3795/FMV302. It is used as a core material to provide rigidity in thin planar components and is a key component in the BPS240 format 2 body panel systems. In this form, VTS243FR is supplied attached to a structural fabric, into which it will infuse during cure. It can also be supplied in sheet form with a lightweight support scrims for general purpose use in constant thickness composite sandwich constructions.

Features & Benefits:

  • 30 days out life at 21°C(70°F)
  • 12 months storage at -18°C (0°F)
  • Available on scrim carriers and structural carbon fiber or glass fiber fabrics
  • Service temperature of 150°C (302°F)
  • Flexible cure characteristics between 65 to 150°C z9149 to 302°F) under vacuum only or higher pressures
  • Self-extinguishes when tested to ISO 3795/FMVS302

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, cured 1 hr at 120°C, 6.2 bar
  • Storage Temperature
  • Maximum Service Temperature, Air
  • Glass Transition Temp, Tg, DMA E' onset
  • Glass Transition Temp, Tg, DMA E' onset Postcured
  • Cure Time
  • Cure Time
  • Cure Time
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.