MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealability

Applications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper coating, Flexible and snack food packaging, Coating of non-porous substrates

Additives: Base resin

Information provided by NOVA Chemicals.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Vapor Transmission, ASTM E96, 90% RH; 30 lb Kraft paper samples with LDPE coating weight of 15 lb/ream
  • Melt Flow, ASTM D1238
  • Neck In, at 1000 ft/min; Neck-in reported is the total of both sides; NOVA Chemicals test method
  • Drawdown, NOVA Chemical test method
  • Coating Weight, TAPPI test method; ASTM D539
  • Hot Tack Strength, Tests done on samples with a coating weight of 12 lb/ream, prepared under the following extrusion coating conditions: Output Rate: 3 lb/hr/in, Melt Temp: 600°F, Die Width: 12 in, Substrate: 40 lb Kraft paper. Mfr reports 450 g per 50 mm (2 in).
  • Heat Seal Strength, ASTM D517, Tests done on samples with a coating weight of 12 lb/ream, prepared under the following extrusion coating conditions: Output Rate: 3 lb/hr/in, Melt Temp: 600°F, Die Width: 12 in, Substrate: 40 lb Kraft paper
  • Melt Temperature, Untreated substrate. Optimum adhesion is obtained at a draw span of about 10 cm.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.