MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Redwood Plastics Redco™ ACETAL HOMOPOLYMER
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Redco™ Acetal brings together the benefits of strength, stiffness, a low coefficient of friction, and dimensional stability providing a versatile and easily machinable material that exceeds the life of many parts that are traditionally metal. Suited for a variety of industries and applications, Redco™ Acetal acts as an electrical insulator, is FDA Approved for food applications, and is an excellent material for use in applications requiring close-tolerances. To minimize delivery times and meet design configurations, Redwood Plastics and Rubber stocks a broad array of Redco™ Acetal sheet and round bar in both white and black. Custom colors and sizes are also available upon request.

Information provided by Redwood Plastics and Rubber

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell M, ASTM D785, At 0.2 in/min loading rate
  • Tensile Strength, ASTM D638
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Fatigue Strength, ASTM D671
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, VS. STEEL
  • Volume Resistivity, ASTM D257, 50% RH
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, short time
  • Dielectric Strength, ASTM D149, short time
  • Dielectric Strength, ASTM D149, short time
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495, burns, no tracking
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.