MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Crucible Compaction Metals Rene 95 Nickel Based Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and low cycle fatigue life. Tens of thousands of high pressure turbine discs and turbine blades retainers made from Crucible Rene 95 are in service on commercial and military airplanes and helicopters worldwide.

Rene 95 is available as either as-HIP preforms or extruded billet. As-HIP parts can range up to 46 inches (1.2 m) in diameter and weighs up to 16,000 lb (7,200 kg). Extruded billet up to 12 inches (.3 m) in diameter is produced from compacts containing up to 8,000 lb (3,600 kg) of powder.

Advantages:

  • High Strength
  • Excellent high temperature creep resistance
  • Extended low cycle fatigue life

Information provided by Crucible Compaction Metals.

Key Words: Powder Metallurgy
Vendors:
Available Properties
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break
  • Reduction of Area
  • Reduction of Area
  • Creep Strength, 0.2% Creep
  • Creep Strength, 0.2% Creep
  • Rupture Strength
  • Rupture Strength
  • Aluminum, Al
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Molybdenum, Mo
  • Nickel, Ni, As Balance
  • Niobium, Nb (Columbium, Cb)
  • Titanium, Ti
  • Tungsten, W
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.