MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
HB Fuller HP008 Hot Melt Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: HP008 is single component hot melt adhesive that cross-links through a chemical reaction with moisture found in the atmosphere and substrates to form a set adhesive. HP008 is a high performance, high green strength grade reactive hot melt with superior adhesion to a variety of substrates. It can be applied using roll coaters, as well as hot melt adhesive guns. It is particularly suited for bonding EPS, PU foam, aluminum, steel, various plastics (PVC, ABS, and SMC), and rubber.

Features and Benefits:

  • High green strength
  • Good heat resistance
  • High adhesion on a variety of substrates
  • High toughness
  • 100% solid

Information provided by H.B. Fuller Company

Vendors:
Available Properties
  • Solids Content
  • Viscosity
  • Tensile Strength, Green
  • Tensile Strength
  • Elongation at Break
  • 2% Secant Modulus
  • Cure Time, Roll Coater Open Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.