MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chesterton 274 Industrial Degreaser
Categories: Fluid; Solvent

Material Notes: Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountered in industrial and marine environments. Industrial Degreaser is designed to be used as received and may be applied by spray, brush or dipping. It is commonly used in commercial parts washers to replace more hazardous solvents. Chesterton 274 Industrial Degreaser has a high flash point and low aromatic content. It offers greatly improved safely compared to conventional petroleum based degreasers.

Features:

  • Dissolves Grease, Oil, Tar and Other Organic Soils
  • High Flash Point
  • Low Aromatic Content
  • Low Odor
  • Low Evaporation Rate
  • Does Not Attack Most Paints and Plastics
  • Safe For Use on All Metals
  • Fast Penetrating Action
  • NSF C1, K1, K2 Registration number 133955 (bulk) and 133949 (aerosol)

Suggested Uses:

  • Degreasing metal parts, equipment, vehicles, floors and other hard surfaces
  • Replacement for kerosene, mineral spirits, chlorinated solvents and naphtha based cleaners and degreasers
  • Use in recirculating and agitated parts washers and dip tanks
  • Degrease surfaces prior to coating
  • Clean equipment before disassembly for maintenance, repair, or machining
  • Remove process oils and other contaminates from in process parts
  • Applications can be found in metal production operations, paint ships, maintenance departments, boiler rooms, repair shops, vehicle and ship yards, among others
  • Cleans non-energized electrical equipment.

    Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Volatiles
  • Vapor Pressure, ASTM D2879
  • Dielectric Strength, ASTM D877
  • Flash Point, ASTM D56, Tag Closed Cup
  • Ignition Temperature, ASTM D2155, Autoignition
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.