MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Angst+Pfister APSOplast® PFA Fluoro plastic
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: General description: PFA is a semi-crystalline copolymer manufactured through the copolymerization of tetrafluorethylen and perfluorovinyl ether. Its melt viscosity is several powers of ten lower than that of PTFE. Unlike the sintered PTFE, PFA can be processed using traditional thermoplastic processing methods such as screw extrusion, transfer moulding, and injection moulding. PFA is also thermo-formable and weldable. The chemical and thermal resistance, anti-adhesion behaviour, and dielectric properties of PFA are largely the same as those of PTFE. In comparison with PTFE, PFA is harder and has better dimensional stability. In addition, the cold flow tendency of PFA is lower.

Characteristics and properties:

  • Excellent service temperature range (long-term exposure to temperatures from –200 to +260 °C)
  • Excellent and universal resistance to chemicals, almost the same as that of PTFE
  • Exceptional mechanical properties, harder and more dimensionally stable than PTFE, with a significantly better bending fatigue strength
  • Extremely high UV- and weather resistance
  • High air permeability
  • Very good dielectric properties
  • Anti-adhesive surface properties
  • Flame-retardant

Information provided by Angst + Pfister

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1
  • Water Absorption at Saturation, DIN EN ISO 62
  • Volume Resistivity, DIN IEC 60023
  • Surface Resistance, DIN IEC 60023
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dielectric Loss Index, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, DIN 53752
  • Melting Point
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.