MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Total PSC 1540(EU) Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact polystyrene such as LACQRENE® 7240. Having high gloss, it is particularly suitable for glossy-layer co-extrusion. In injection molding, 1541 possesses low viscosity at high shear rate. It does combine excellent fluidity with a higher softening point that 1810/1811.

Application

Dairy sheet, Cups, Coextrusion crystal, Boxes, Petra dishes, Medical products, Office equipment - e.g. filling trays, CD boxes, Pen bodies, Internal fridge parts.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines. This product was previously known as LACQRENE®

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage
  • Melt Flow, ISO 1133H
  • Hardness, Rockwell L, ISO 2039-2
  • Tensile Strength at Break, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Surface Resistivity per Square, ISO IEC93
  • Dielectric Strength
  • CTE, linear
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2B, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2A, Unannealed
  • Vicat Softening Point, ISO 306B50, 50N (T° increase = 5°C/h)
  • Vicat Softening Point, ISO 306A50, 10N (T° increase = 50°C/h)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.