MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Alfa Chemistry Materials Cerium (III) Sulfide
Categories: Ceramic; Sulfide/Chalcogenide

Material Notes: Cerium (III) Sulfide Powder is one of the sulfides of cerium, the chemical formula is Ce2S3. ?-Ce2S3 is a brownish-red solid, and its color changes to orange when it is mixed with alkali metals. Cerium(III) Sulfide Powder was synthesized via the sulfurization of ceria (CeO2) powder using carbon disulfide gas.

Applications: Cerium sesquisulfide (Ce2S3) has many applications stemming from its high temperature stability and electronic configuration. Cerium (III) Sulfide Powder is used in laboratory researches. It is a semiconductor with a band gap of 2.06 eV and a high Seebeck coefficient. It can be used as a high temperature pigment due to its bright red color. Cerium sesquisulfide is also an essential compound that is often required for the synthesis of
cerium monosulfide.

Molecular Formula: Ce2S3

Alfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors:
Available Properties
  • Density
  • Solubility in Water, Insoluble
  • Molecular Weight
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.