General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transparency properties. Main Applications: High transparency soft/hard sheet, hoses, wrapping film and innoxious film. CAS No: 9002-86-2 Information provided by LG Chemical |