MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded; Polystyrene (PS)

Material Notes:

Features:

  • High clarity
  • Styrenic processing advantages
  • Excellent property retention after ETO and gamma sterilization
  • Excellent indoor light stability
  • High elongation and ductility
  • Applications:

  • Appliances
  • Office accessories
  • Long-lasting modular displays
  • Housewares
  • Toys
  • General information about ZYLAR®: ZYLAR® acrylic copolymers are The Clear Alternative to polycarbonate, PETG, impact acrylic and clear ABS for applications that demand clarity and toughness and enhanced processing productivity. ZYLAR is a cost effective alternative in injection molding applications, with over 15 years of proven performance.

    ZYLAR has proven performance in a variety of applications, including medical, floor care, appliances, consumer goods, office accessories and supplies, pens and mechanical pencils, commercial paper towel dispensers, point of purchase displays, cosmetics packaging, toys, electronics packaging, housewares, consumer & industrial, and other applications.

    ZYLAR® acrylic copolymers provide value through enhanced performance, manufacturing productivity, ease of processing, and potential for capital avoidance through utilization of existing (styrenics) equipment and tooling.

    Performance Attributes:

    • Crisp clarity
    • Outstanding practical toughness and ductility
    • Balance of toughness and clarity
    • Easily decorated
    • Can be printed, hot stamped or metalized.
    • Gamma, Eto and E-beam sterilizable
    • Can be bonded to flexible PVC
    • Alcohol and lipid resistance
    • Resistance to most industrial and commercial cleaners
    • Resistance to most household cleaners
    • Resistant to most food additives
    • Residential dishwasher safe - top rack
    • Secondary operations include sonic welding, hotplate welding, ultrasonic bonding and adhesive bonding
    • Over-molding capability
    Product Capabilities
    • Antistatic and indoor UV grades available
    • Available in natural and pre-colored
    • Color matching capabilities

    Customer Productivity & Processing

    • 5 to 25% density advantage means more parts per pound of resin
    • Faster cycle time
    • Reduced energy and labor costs associated with processing
    • Lower processing temperatures by as much as 150F
    • No drying
    • Styrenic processing
    • Better thermal stability
    • More usable regrind and no black specs
    • Product consistency, color consistency
    • Easily colored at the press
    • Easy flow
    • Able to utilize existing tooling for PC, clear ABS, impact acrylic, PETG, polyesters, propionate (CAP), PVC and other polymers

    Information provided by Nova Chemicals

    This specific grade was discontinued prior to the Styrolution acquision of the Zylar® product line.

    Vendors:
    Available Properties
    • Specific Gravity, ASTM D792
    • Linear Mold Shrinkage, ASTM D955
    • Melt Flow, ASTM D1238, Condition G
    • Hardness, Rockwell R, ASTM D785
    • Tensile Strength, Yield, ASTM D638
    • Elongation at Break, ASTM D638
    • Tensile Modulus, ASTM D638
    • Flexural Strength, ASTM D790
    • Flexural Modulus, ASTM D790
    • Izod Impact, Notched, ASTM D256, reverse notched
    • Izod Impact, Unnotched, ASTM D256
    • Gardner Impact, ASTM D5420, Geometry GB
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
    • Vicat Softening Point, ASTM D1525
    • Refractive Index, ASTM D542, nD
    • Haze, ASTM D1003
    • Transmission, Visible, ASTM D1003
    • Rear Barrel Temperature
    • Middle Barrel Temperature
    • Front Barrel Temperature
    • Melt Temperature
    • Mold Temperature
    • Back Pressure
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.