MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Parker Chomerics CHO-BOND® 1121 General Purpose Adhesive-Sealant Silver Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Xylene-free version of CHO-BOND 1038; rec. bond line thickness: > 0.18 mm; primer promotes adhesion CHO-BOND® 1121 is an electrically conductive, one-component silicone adhesive-sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposure to atmospheric moisture and contains no acetic acid or other corrosive agents. Cured CHO-BOND 1121 remains flexible and conductive at temperatures from -55°C to 125°C. Uncured CHO-BOND 1038 is a smooth, nonflowing paste that may be knife-spread or applied directly to a vertical surface. CHO-BOND 1121 forms a cured skin within two minutes after exposure to atmospheric moisture and therefore must be tooled within this time period. A full cure is obtained after room temperature aging at 50% relative humidity for one week. In many cases, a good set is obtained within 8 hours. Priming the substrate with CHO-BOND 1086 is recommended.

Typical Applications: Sealing enclosure seams; airframe gap sealing; connector shielding.

Information provided by Chomerics

Vendors:
Available Properties
  • Specific Gravity
  • Volatile Organic Compounds (VOC) Content
  • Thickness
  • Shear Strength, Lap
  • Volume Resistivity
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.