Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electrical equipment. Applications: Compound designed specially for sealing SF6 gas in electrical distribution equipment, i.e. medium & high voltage switchgear at low temperatures. The specially selected fillers used in this compound impart excellent electrical non-conductive properties to the rubber. |