MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay METLBOND® 1515-3 Film Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Metlbond® 1515-3 and Metlbond 1515-3 MHT are 350°F (177°C) curing modified epoxy supported film adhesives. Metlbond 1515-3 can also be cured at 250°F (121°C). Its maximum continuous service temperature range is 275°F to 320°F (135°C to 160°C). Metlbond 1515-3 is available in medium- and high-tack (HT) versions which give the same mechanical and physical properties. Metlbond 1515-3 is commonly used for BMS 5-154 metal-to-metal and composite bonding and BMS 8-341 cosmetic surfacing.

Features & Benefits:

  • Industry standard for composite bonding and surfacing applications
  • Designed for co-curing, secondary bonding, co-bonding of composite materials
  • Provides excellent surfacing characteristics
  • Good resistance to pre-cure humidity
  • Available in a variety of weights and carriers
  • Bonds metal-to-metal, metal-to-core and composites
  • Co-cures with most 350°F (177°C) curing prepregs
  • Shelf life of 12 months at 0°F (-18°C) or 1 month at 40°F (4°C)
  • Shop life of 15 days at 75°F (24°C)
Applications:
  • Metal-to-metal bonding
  • Composite bonding
  • Cosmetic surfacing

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Volatiles
  • Tensile Strength, Metal-to-Honeycomb Flatwise
  • Tensile Strength, Metal-to-Honeycomb Flatwise
  • Tensile Strength, Honeycomb Flatwise, Grade 03: 0.0325 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 03: 0.0325 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 08: 0.08 lb/ft2
  • Tensile Strength, Metal-to-Honeycomb Flatwise
  • Tensile Strength, Honeycomb Flatwise, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 05: 0.05 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 03: 0.0325 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 08: 0.08 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 08: 0.08 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 05: 0.05 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 05: 0.05 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 08: 0.08 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 05: 0.05 lb/ft2
  • Tensile Strength, Honeycomb Flatwise, Grade 03: 0.0325 lb/ft2
  • Tensile Strength, Composite-to-Honeycomb Flatwise
  • Tensile Strength, Composite-to-Honeycomb Flatwise
  • Tensile Strength, Composite-to-Honeycomb Flatwise
  • Tensile Strength, Metal-to-Honeycomb Flatwise
  • Tensile Strength, Metal-to-Honeycomb Flatwise
  • Shear Strength, Sandwich Beam, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 05: 0.05 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 08: 0.08 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 08: 0.08 lb/ft2
  • Shear Strength, Composite-to-Composite Double Lap, Substrate: Carbon epoxy composite per BMS 8-212
  • Shear Strength, Sandwich Beam, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 05: 0.05 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 08: 0.08 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 05: 0.05 lb/ft2
  • Shear Strength, Sandwich Beam, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Metal-to-Metal Lap, Substrate: 2024 T3 aluminum, no primer Tested at 270°F (132°C)
  • Shear Strength, Composite-to-Composite Double Lap, Substrate: Carbon epoxy composite per BMS 8-212
  • Shear Strength, Double Lap, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Grade 05: 0.05 lb/ft2
  • Shear Strength, Metal-to-Metal Double Lap, Substrate: 2024 T3 aluminum, no primer
  • Shear Strength, Double Lap, Grade 08: 0.08 lb/ft2
  • Shear Strength, Composite-to-Composite Double Lap, Substrate: Carbon epoxy composite per BMS 8-212
  • Shear Strength, Metal-to-Metal Lap, Substrate: 2024 T3 aluminum, no primer Tested at 270°F (132°C)
  • Shear Strength, Metal-to-Metal Double Lap, Substrate: 2024 T3 aluminum, no primer
  • Shear Strength, Double Lap, Grade 08: 0.08 lb/ft2
  • Shear Strength, Metal-to-Metal Lap, Substrate: 2024 T3 aluminum, no primer Tested at 270°F (132°C)
  • Shear Strength, Double Lap, Grade 08: 0.08 lb/ft2
  • Shear Strength, Double Lap, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Grade 05: 0.05 lb/ft2
  • Shear Strength, Double Lap, Grade 05: 0.05 lb/ft2
  • Shear Strength, Double Lap, Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Grade 08: 0.08 lb/ft2
  • Shear Strength, Double Lap, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 05: 0.05 lb/ft2
  • Shear Strength, Double Lap, Exposure Prior to Testing: 14 days at 160°F (71°C) and 100% R.H., Grade 08: 0.08 lb/ft2
  • Shear Strength, Double Lap, Exposure Prior to Testing: 1000 hours at 160°F (71°C) and 100% R.H., Grade 08: 0.08 lb/ft2
  • Shear Strength, Double Lap, Exposure Prior to Testing: 1000 hours at 160°F (71°C) and 100% R.H., Grade 03: 0.0325 lb/ft2
  • Shear Strength, Double Lap, Grade 05: 0.05 lb/ft2
  • Shear Strength, Metal-to-Metal Lap, Substrate: 2024 T3 aluminum, no primer Tested at 270°F (132°C)
  • Shear Strength, Metal-to-Metal Double Lap, Substrate: 2024 T3 aluminum, no primer
  • Shear Strength, Metal-to-Metal Lap, Substrate: 2024 T3 aluminum, no primer Tested at 270°F (132°C)
  • Shear Strength, Double Lap, Exposure Prior to Testing: 1000 hours at 160°F (71°C) and 100% R.H., Grade 05: 0.05 lb/ft2
  • Shear Strength, Composite-to-Composite Double Lap, Substrate: Carbon epoxy composite per BMS 8-212
  • Shear Strength, Composite-to-Composite Double Lap, Substrate: Carbon epoxy composite per BMS 8-212
  • Shear Strength, Metal-to-Metal Double Lap, Substrate: 2024 T3 aluminum, no primer
  • Shear Strength, Metal-to-Metal Double Lap, Substrate: 2024 T3 aluminum, no primer
  • Peel Strength, Metal-to-Metal Bell
  • Peel Strength, Metal-to-Metal Bell
  • Peel Strength, Metal-to-Metal Bell
  • Peel Strength, Metal-to-Metal Bell
  • Peel Strength, Metal-to-Metal Bell
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, G’ knee by dynamic mechanical analysis
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.