MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Morgan Advanced Ceramics Mineral Fiber Paper 400-LS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Mineral Fiber, Utility grade fiber. 400-LS paper is produced from premium, high quality mineral fibers and organic binders in a unique paper making process. This utility grade paper is noted for good tensile strengths, outstanding handling characteristics, and good insulating values, while being very cost effective. The 400-LS product is a very clean, low shot paper with a high quality surface texture and low thermal conductivity value. 400-LS paper can be die-cut in accordance with customer specifications in a variety of shapes and sizes.

Applications:

  • High temperature gasketing
  • Automotive heat shields and muffler insulation
  • Ladle refractory back up
  • Glass tank refractory back up
  • Appliance/radiant heater insulation
  • Back up for aluminum troughs and metal transfer parts
  • Back up lining for aluminum holding furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Loss On Ignition
  • Tensile Strength, fired
  • Tensile Strength
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Melting Point
  • Maximum Service Temperature, Air
  • Al2O3
  • CaO
  • Other
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.