MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Aluminum 7175-T736; 7175-T7365x (extended High Temperature Data)
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97175; Aluminium 7175-T736; Aluminium 7175-T7365; AA7175-T7365
Vendors:
Available Properties
  • Density, AA; Typical
  • Hardness, Brinell, 500 kg load with 10 mm ball
  • Hardness, Knoop, Converted from Brinell Hardness Value
  • Hardness, Rockwell A, Converted from Brinell Hardness Value
  • Hardness, Rockwell B, Converted from Brinell Hardness Value
  • Hardness, Vickers, Converted from Brinell Hardness Value
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Ultimate, Die forging
  • Tensile Strength, Yield
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Tensile Strength, Yield, Die forging
  • Elongation at Break, In 5 cm
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Elongation at Break, Die forging
  • Tensile Modulus, Compressive Modulus is about 2% higher
  • Poissons Ratio, Estimated from trends in similar Al alloys.
  • Fatigue Strength
  • Fracture Toughness, Die Forgings; T-L; S-L
  • Fracture Toughness, Hand Forgings; S-L
  • Fracture Toughness, average; Hand Forgings; S-L
  • Fracture Toughness, Hand Forgings; T-L
  • Fracture Toughness, average; Die Forgings; T-L; S-L
  • Fracture Toughness, average; Hand Forgings; T-L
  • Fracture Toughness, Die Forgings; L-T
  • Fracture Toughness, K(IC) in S-L Direction
  • Fracture Toughness, Hand Forgings; L-T
  • Fracture Toughness, average; Die Forgings; L-T
  • Fracture Toughness, K(IC) in T-L Direction
  • Fracture Toughness, average; Hand Forgings; L-T
  • Fracture Toughness, K(IC) in L-T Direction
  • Shear Modulus, Estimated from similar Al alloys.
  • Shear Strength, Calculated value.
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear, AA; Typical; average over range
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, AA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Homogenization may raise eutectic melting temperature 20-40°F but usually does not eliminate it.
  • Solidus, AA; Typical
  • Liquidus, AA; Typical
  • Annealing Temperature
  • Solution Temperature, must be preceded by soak at 890 to 905°F; quench from lower temperature
  • Aging Temperature
  • Aluminum, Al, As remainder
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Other, each
  • Other, total
  • Silicon, Si
  • Titanium, Ti
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.