MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: RT/duroid® 5880LZ filled PTFE composites are designed for exacting stripline and microstrip circuit applications. The unique filler results in a low density, lightweight material for high performance weight sensitive applications

The very low dielectric constant of RT/duroid 5880LZ laminate is uniform from panel to panel and is constant over a wide frequency range. Its low dissipation factor extends the usefulness of RT/duroid 5880LZ to Ku-band and above.

RT/duroid 5880LZ laminates are easily cut, sheared and machined to shape. They are resistant to all solvents and reagents, hot or cold, normally used in etching printed circuits or in plating edges and holes.
Available with a range of copper cladding options.

Features:

  • Lowest dielectric constant available
  • Low Z-axis CTE
  • Lightweight / low density
  • Uniform electrical properties over a wide frequency range
  • Lead free process compatible

Typical Applications:

  • Airborne Antenna Systems
  • Lightweight feed networks
  • Military Radar Systems
  • Missile Guidance Systems
  • Point to Point Digital Radio Antennas

Information provided by Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D792
  • Moisture Absorption at Equilibrium, ASTM D570
  • Thickness, Range of thicknesses available
  • Outgassing - Total Mass Loss, ASTM E595, TML
  • Outgassing - Total Mass Loss, ASTM E595, WVR
  • Collected Volatile Condensable Material, ASTM E595
  • Peel Strength, IPC-TM-650 2.4.8, Copper
  • Volume Resistivity, IPC 2.5.17.1, Condition A
  • Surface Resistance, IPC 2.5.17.1, Condition A
  • Dielectric Constant, IPC-TM-650 2.5.5.5, Z direction; Process
  • Dielectric Constant, Differential Phase Length Method, Z direction; Design
  • Dielectric Strength, IPC-TM-650 2.5.6.2
  • Dissipation Factor, IPC-TM-650 2.5.5.3, Z direction
  • Dissipation Factor, IPC-TM-650 2.5.5.5, Z direction
  • CTE, linear, IPC-TM-650 2.4.41, Z-Direction
  • CTE, linear, IPC-TM-650 2.4.41, Y-Direction
  • CTE, linear, IPC-TM-650 2.4.41, X-Direction
  • Specific Heat Capacity, calculated
  • Thermal Conductivity, ASTM C518, Z direction
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.