MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Formosa Plastics Formolene® HP4306 Pipe HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: High Density Hexene Copolymer

Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for larger diameter and thick wall pipes where excellent melt strength is required, but can be used successfully on all diameters and wall thicknesses. It has good long-term hoop strength performance, very high melt strength, and outstanding toughness even at low temperatures. Formolene® HP 4306 meets all requirements of ASTM D4976 – PE 235. When blended with the approved color concentrates, Formolene® HP4306 has a cell class of 345464C per ASTM D3350-05, is listed by PPI as a PE3608 material with HDB's of 1,600 psi @ 73°F and 800 psi @ 140°F and meets the requirements of NSF Standard 14/61 for use with potable water. Formolene® HP4306 also qualifies as a PE3408 material under the old ASTM D3350-02a and PPI standards. Formolene® HP4306 also qualifies as a PE80 material per ISO 9080.

Applications: Potable Water; Oil and Gas Gathering and Distribution; Chemical, Industrial and Mining; Sewer

Information provided by Formosa Plastics Corporation, USA

Vendors:
Available Properties
  • Density, ASTM D1505, Natural
  • Density, ASTM D1505, Black
  • ESCR 100% Igepal®, ASTM D1693, Condition A, B, C, F50
  • Melt Flow, ASTM D1238, Condition E
  • High Load Melt Index, ASTM D1238, Condition F
  • PENT, ASTM F1473, Slow Crack Growth
  • Tensile Strength at Break, ASTM D638, 2" (50mm) per min, Type IV
  • Tensile Strength, Yield, ASTM D638, 2" (50mm) per min, Type IV
  • Elongation at Break, ASTM D638, 2" (50mm) per min, Type IV
  • Flexural Modulus, ASTM D3350
  • Flexural Modulus, ASTM D790
  • Brittleness Temperature, ASTM D746
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Formosa Plastics Corporation, USA

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.