An ethylene-based hexene plastomer produced by Exxon Chemical's EXXPOL technology. This resin is designed primarily for use in blends with polyolefins to improve the heat sealing performance and toughness in film application. Data for film properties below based on 2 mil film.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer