MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond Supreme 11AOHT Thermally Conductive, Heat Resistant Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • High thermal conductivity
  • Superior electrical insulation
  • Room temperature curing
  • High thermal conductivity
  • Superior electrical insulation
  • Room temperature curing
Product Description: Master Bond Supreme 11AOHT is a two component epoxy resin system for high performance bonding and sealing. It is formulated to cure at room temperature or more rapidly at elevated temperatures with a convenient one to one mix ratio by weight or volume. Its most outstanding features include high thermal conductivity, excellent electrical insulation properties and temperature resistance up to +400°F. Supreme 11AOHT is a “toughened” system which enables it to withstand rigorous thermal cycling and makes it well suited for bonding dissimilar substrates. It has excellent adhesion to most metals, ceramics, glass and vulcanized rubbers as well as many plastics. Additionally, the toughness imparts high shear and peel strengths. Its chemical resistance profile includes water, oil and fuels. Both Parts A and B are colored off-white. Master Bond Supreme 11AOHT is widely used in electronic, electro-optic, aerospace and specialty applications where high strength, excellent thermal transfer properties, and high temperature resistance are required.

Product Advantages:

  • Convenient one to one mix ratio by weight or volume
  • Versatile cure schedules; ambient temperature cures or faster elevated temperature cures as required
  • High shear and peel strengths to a wide variety of substrates
  • Toughened system, can withstand rigorous thermal Cycling
  • High thermal conductivity with exceptional electrical insulation properties
  • Thermally stable up to +400°F with good thermal cycling properties
  • Exceptionally good dimensional stability

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap, Aluminum to Aluminum
  • Peel Strength, aluminum to aluminum
  • Volume Resistivity
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.