MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Schmolz + Bickenbach 416RS Stainless Steel Bar
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanced to provide the optimum machining characteristics for gun barrel drilling and reaming - while also offering the optimal combination of high tensile strength and good toughness to withstand the typical chamber pressures when fired. Ugitech 416RS comes pre-hardened to HRc 26/32, but can be produced to the specific hardness requirements. The precision finished bars are properly stress relieved to provide the superb straightness necessary to avoid movement during processing, while also offering good corrosion resistance which will reduce fouling and provide a durable finish. Ugitech’s 416RS is 100% ultrasonic tested. The mill’s stringently controlled production will deliver heat to heat consistency. Every step is monitored from melt, rolling, heat treatment, cold finishing, final bar inspection, and Packaging

Stress Relieving (Heat Treatment): Heat and hold for 50°F – 100°F (10°C to 40°C) below tempering temperature of 4-7 hours, slow cool

Hardening (Heat Treatment): Should be performed at 1750°F (950°C), followed by air or oil quenching.

Information provided by Schmolz + Bickenbach

Key Words: ASTM A370; A484; A582; E381; AMS 2315
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Turned Bars
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Turned Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Yield, Turned Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Elongation at Yield, Turned Bars
  • Elongation at Yield, Cold Drawn Bars
  • Reduction of Area, Cold Drawn Bars
  • Reduction of Area, Turned Bars
  • Tensile Modulus
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, Sub-critical anneal
  • Annealing Temperature, Softest properties
  • Hot-Working Temperature, Slow heating
  • Hot-Working Temperature, Forging range
  • Hot-Working Temperature, Then more rapidly
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.