MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
China-Yixing Longly Refractories Zirconia Ceramics
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing, isostatic pressing and hot pressing. The fine grain size allows for extremely smooth surfaces. Meanwhile Zirconia has low thermal conductivity and is an oxygen-ion conductor above 600°C, which could be used as oxygen sensors and high temperature fuel cells.

Compared with alumina ceramics, they have higher abrasion resistance, flexibility, chemical stability, and corrosion resistance. LONGLY's Zirconia products are high temperature resistant, hard, insulated, wear resistant, anti-split, high pressure resistant, particularly tough and without use of any auxiliary lubricant, which are most suitable for harsh environment. We could manufacture and machine various precision ceramic structural parts according to customer request. Main products consist of grinding ball, nozzle, ball valve, ball seat, zirconia molds, optical fiber base pin, optical fiber ferrule, wire drawing film, sealing ring and other wear-resistant parts.

Applications: Widely used in metallurgical, electrical, electronic, automotive, pneumatic components, machinery, chemical, textile and other fields.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Particle Size, grain size; 400lambda - 800lambda
  • Vickers Microhardness, (kg/mm2)
  • Modulus of Elasticity
  • Fracture Toughness
  • Dielectric Strength, Insulating Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • ZrO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
China-Yixing Longly Refractories Co. Ltd

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.