MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Syensqo (Solvay Specialty Polymers) Udel® P-3703 PSU, Transparent
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Transparent, high flow for injection molding

Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly greater tendency to stress crack in some aggressive environments.

Udel® polysulfone is a tough, rigid, high-strength thermoplastic that maintains its properties at temperatures from -101°C to 149°C (-150°F to 300°F). The heat deflection temperature at 1.8 MPa (264 psi) is 174°C (345°F). For most purposes, this resin is suitable for continuous use up to 149°C (300°F). The material is resistant to oxidation and hydrolysis and withstands prolonged exposure to high temperatures and repeated sterilization. Udel polysulfone is highly resistant to mineral acids, alkali and salt solutions. The resistance to detergents and hydrocarbon oils is good, but it will be attacked by polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons.

Electrical properties of Udel polysulfone are stable over a wide temperature range and after immersion in water or exposure to high humidity.

- Natural: Udel® P-3703 NT 11

Applications: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Parts; Microwave Cookware; Piping; Plumbing Parts; Valves/Valve Parts

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Chemical Resistant; Food Contact Acceptable; Good Toughness; High Flow; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Tensile Impact Strength, ASTM D1822
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Flammability, UL94
  • Flammability, UL94
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  • Shot Size
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.