MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Park Aerospace Nelco® N5000 BT Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and commercial boards requiring not only close thicknesstolerance, but also the ability to withstand the stress of multiple soldering excursions and repeated chemical exposure.

Key Features and Benefits:

  • BT resin chemistry
  • Excellent Reliability and Performance
  • CAF Resistant
  • Wide processing latitude

Applications/Qualifications:

  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • MCM-Ls
  • Direct Chip Attach
  • Wireless Communications
  • High Density Interconnects
  • RoHS Compliant
  • Meets IPC-4101/30 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors:
Available Properties
  • Density, 50% Resin Content; Internal Method
  • Water Absorption, IPC-TM-650.2.6.2.1
  • Modulus of Elasticity, ASTM D3039, Y
  • Modulus of Elasticity, ASTM D3039, X
  • Poissons Ratio, ASTM D3039, Y
  • Poissons Ratio, ASTM D3039, X
  • Peel Strength, IPC-TM-650.2.4.8.2a, at elevated temperature
  • Peel Strength, IPC-TM-650.2.4.8, after solder float
  • Peel Strength, IPC-TM-650.2.4.8, after exposure to process solutions
  • Volume Resistivity, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Volume Resistivity, IPC-TM-650.2.5.17.1, E - 24/125
  • Surface Resistance, IPC-TM-650.2.5.17.1, C - 96/35/90
  • Surface Resistance, IPC-TM-650.2.5.17.1, E - 24/125
  • Dielectric Constant, IPC-TM-650.2.5.5.5, Stripline
  • Dielectric Constant, IPC-TM-650.2.5.5.5, Stripline
  • Dielectric Constant, Split Post Cavity
  • Dielectric Constant, IPC-TM-650.2.5.5.9, RF Impedance
  • Dielectric Strength, IPC-TM-650.2.5.6.2
  • Dielectric Breakdown, IPC-TM-650.2.5.6
  • Dissipation Factor, IPC-TM-650.2.5.5.5, Split Post Cavity
  • Dissipation Factor, Stripline
  • Dissipation Factor, IPC-TM-650.2.5.5.5, Stripline
  • Arc Resistance, IPC-TM-650.2.5.1
  • CTE, linear, IPC-TM-650.2.4.41, X/Y
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24c, TMA
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.25c, DSC
  • Glass Transition Temp, Tg, IPC-TM-650.2.4.24.3, DMA (Tan d Peak)
  • Decomposition Temperature, IPC-TM-650.2.4.24.6, 5% weight loss; TGA
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Park Aerospace, former Park Electrochemical Corp.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.