MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Borealis BC650MO Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features high impact strength, high thermal stability and very good processability. As all polypropylenes, this grade shows excellent stresscracking and chemical resistances. This grade is characterized by combination of good stiffness, good creep resistance and very high impact strength even at low temperatures. This grade is mildly nucleated to maximize the mechanical stiffness. The additive formulation provides a smooth demolding. Nucleation, good flow properties and high stiffness create a high potential for cycle time reduction. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring problems. Applications: crates and boxes, pallets, technical parts, bottle trays, and luggage.

Information provided by Borealis AG

Vendors:
Available Properties
  • Density, ISO 1183
  • Linear Mold Shrinkage
  • Melt Flow, ISO 1133
  • Hardness, Rockwell R, ISO 2039-2
  • Tensile Strength, Yield, ISO 527-2, 50mm/min
  • Elongation at Yield, ISO 527-2, 50mm/min
  • Tensile Modulus, ISO 527-2, 1mm/min
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Puncture Energy, ISO 6603-2
  • Puncture Energy, ISO 6603-2
  • Puncture Energy, ISO 6603-2
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2
  • Melt Temperature
  • Mold Temperature
  • Hold Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.