MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Wacker Powersil® 3525 MH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: POWERSIL® 3525 MH silicone rubber is a one component, ready to use, addition-curing compound that cures to an electrical insulating, highly erosion resistive silicone elastomer. POWERSIL® 3525 MH shows fast curing in comparison to conventional silicone rubber. Curing time is reduced by (30 … 50) % depending on the wall thickness and on the available machinery and runner system. No peroxide decomposition products are released while curing.

Special features:

  • easy demolding
  • excellent dielectric properties
  • high arcing and tracking resistance
  • no unpleasant smell caused by peroxides
  • no inhibition by oxygen
Application: POWERSIL® 3525 MH is especially designed for T&D applications. Because of its excellent mechanical properties POWERSIL® 3525 MH is prone for use in “cable accessories” applications. Especially thick walled articles can take advantage of the fast curing material.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN 53479
  • Hardness, Shore A, ISO 868
  • Tensile Strength at Break, ISO 37
  • Elongation at Break, ISO 37
  • Tear Strength, ASTM 624 B
  • Volume Resistivity, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243
  • Dissipation Factor, IEC 60250
  • Arc Resistance, IEC 61621
  • Cure Time, post-cured 4hr at 150°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.