MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dover Chemical MAYSOL HOSS Semi-synthetic Super Concentrate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: MAYSOL HOSS is a premium high oil content semi-synthetic super concentrate for machining and grinding of ferrous and non-ferrous alloys. It is ideally suited for manufacturing operations that want a single fluid to machine a variety of metals. MAYSOL HOSS, as received, is to be added to water at a 50/50 ratio. Never in reverse; adding water to the product. After this initial water let-back, it can be further reduced at your customer’s site to the desired final concentration – typically, grinding (3-5%), and machining (4-8%) Advantages and Benefits: Versatile fluid suitable for a wide range of applications on multiple metals. Non-chlorinated Extreme Pressure lubrication extends tool life and improves finishes. Exhibits almost 50% higher buffer property compared to other semi-synthetics; i.e. better pH stability. Excellent rust protection down to 2%. No included defoamers; possess relatively low foam property

Information provided by DoverChem

Vendors:
Available Properties
  • Specific Gravity, 60/60°F
  • pH, 5% dilution
  • Total Acid Number, [mgKOH/g]
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.