Product Description: Pibiflex 4568T is a heat stabilized, hydrolysis resistant and nominal 45 Shore D thermoplastic polyester elastomer with a high melting point. Preliminary datasheet. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Additive: Hydrolysis Resistant; Lubricant Features: Good Heat Resistance; Hydrolysis Resistant; Lubricated Automotive Specifications Information provided by Celanese |