MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Covestro Bayfill® EA 2003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Bayfill EA 2003 is a low-density, semirigid polyurethane foam system designed for automotive interior applications.

Properties / Applications: Bayfill EA 2003 is a low-density, semirigid polyurethane foam system designed for automotive interior applications. It produces a friable foam which has the ability to absorb more energy in applications where space is limited. The Bayfill EA system is an excellent choice where occupant impact protection above the vehicle beltline is required or desired. Foams made with Bayfill EA 2003 can be incorporated into vehicle headliners and pillar covers for improved occupant protection in collisions. Because such foam is friable, it should be considered a sacrificial energy absorber and should be replaced after damage by an impact. The Bayfill EA 2003 system is supplied as two components. Component A is a polymeric diphenylmethane diisocyanate (PMDI) and Component B, is a polyether polyol system. As with any product, use of Bayfill EA 2003 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors:
Available Properties
  • Specific Gravity, Polyol Blend (Component B)
  • Specific Gravity, Isocyanate (Component A)
  • Viscosity, Isocyanate (Component A)
  • Viscosity, Polyol Blend (Component B)
  • Compressive Strength, ASTM D1621, 10% compression, Density 64 kg/m3
  • Compressive Strength, ASTM D1621, 50% compression, Density 64 kg/m3
  • Compressive Strength, ASTM D1621, 70% compression, Density 80 kg/m3
  • Compressive Strength, ASTM D1621, 50% compression, Density 80 kg/m3
  • Compressive Strength, ASTM D1621, 70% compression, Density 64 kg/m3
  • Compressive Strength, ASTM D1621, 10% compression, Density 96 kg/m3
  • Compressive Strength, ASTM D1621, 50% compression, Density 96 kg/m3
  • Compressive Strength, ASTM D1621, 70% compression, Density 80 kg/m3
  • Compressive Strength, ASTM D1621, 70% compression, Density 96 kg/m3
  • Flash Point, Polyol Blend (Component B)
  • Flash Point, Isocyanate (Component A)
  • Mold Temperature
  • Gel Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.