MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chesterton 415 Concrete Sealer  (discontinued **)
Categories: Polymer; Adhesive

Material Notes: Chesterton® 415 Concrete Sealer is a high gloss, fast penetrating coating which forms a polymeric seal over surfaces to which it is applied. When used on porous surfaces such as concrete floors, walls, pavement, and structures, it reduces dusting, deterioration and damage due to weathering. Surfaces are left with a tough, beautifully lustrous finish that is resistant to most chemicals, water, oil and grease. 415 Concrete Sealer is resistant to mildew and bacteria and will not discolor with age. Chesterton 415 Concrete Sealer is the easy to use coating for concrete surfaces. While most conventional coatings require the concrete surface to be neutralized by acid etching prior to application, this is not necessary when using 415 Concrete Sealer. Just clean and degrease and the surface is ready for coating. Under most environmental conditions, the coating is dry and ready for traffic in three to four hours.

Features:

  • Dries in 3-4 hours
  • Can be used on new and old concrete
  • No acid etching required before use
  • Protects against mildew, bacteria, moisture, acid, rain and pollution
  • Clear, lustrous coating
  • Eliminates dusting
  • No peeling or flaking
  • Can be applied to damp concrete
  • Makes surfaces easy to clean
  • NSF R2 – Registration number 134009

Applications: Use as a polymer seal to reduce dusting, deterioration and weathering on all concrete, cement blocks, stucco, Terrazzo, bricks, stone and other masonry surfaces; use on floors, walls, buildings, bridges, sidewalks and other structures.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity
  • Dry Time, Touch
  • Dry Time, Recoat
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.