MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
3M Dyneon™ Dynamar™ FX 5920B Polymer Processing Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Fluoropolymer, TS

Material Notes: Dynamar polymer processing additive FX 5920B is designed for those who want to determine processing additive levels by x-ray fluoresence. FX 5920B utilitizes FX 5920A processing additive technology. FX 5920B contains 10% of a food grade Barium Sulfate as a tracing additive. By quantifying the Barium level via known x-ray fluoroescence techniques one can easily calculate the amount of polymer processing additive that has been incorporated into the plastic.

Features and Benefits

  • Broadens extrusion capabilities of polyolefin resins
  • Designed for x-ray fluoroscence analytical test methods
  • Ideal for use in polyolefin resins containing antiblocking agents, pigments, and other inorganic additives
  • Reduces or eliminates melt fracture
  • Reduces or eliminates die build-up
  • Lowers apparent melt viscosity
  • For use at very low levels
  • Free-flowing fluoropolymer based processing aid
  • Can offer performance and cost advantages

Information provided by Dyneon, A 3M Company

Vendors:
Available Properties
  • Bulk Density
  • Additive Loading, BaSO4
  • Particle Mesh Size
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dyneon, Division of 3M

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.