MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Exceed™ 2305 MI Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Enable™ performance PE polymers allows film converters to further enhance their business with more stable operations, improve line output and down gauging — in one single polymer for mono- and coextrusion operations.  Enable™ 2305 resins are ethylene 1-hexene copolymers.  This polymer offers an outstanding balance between processing and film properties, including tensile, impact and puncture. Easier processing and excellent properties lead to significant high pressure LDPE replacement in many applications, yet with superior draw down and enhanced toughness.  Enable™2305 resins are available with and without antiblock.  TnPP is not intentionally added to Enable™2305 resins.   

Availability:   North America.  

Additive:  antiblock: 2000ppm; slip: no; processing aid: yes; thermal stabilizer: yes.

Applications:  agricultural film, food packaging, multilayer packaging film, shrink film, blown film, form fill and seal packaging, stand up pouches, heavy duty bags, collation shrink, lamination film.  Forms:  pellets.

Information provided by ExxonMobil.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Puncture Energy, ExxonMobil Method
  • Elmendorf Tear Strength MD, ASTM D1922
  • Elmendorf Tear Strength TD, ASTM D1922
  • Dart Drop Test, ASTM D1709A
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Melting Point, ExxonMobil Method, Peak
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, @ 45°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.