MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman 9921P PET Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia, Brazil, Chile, Colombia, Mexico, Paraguay, Peru, Uruguay and Venezuela. Voridian PET 9921P will be used primarily for thick wall applications such as refill bottles for water and carbonated soft drinks.

Applications/Uses

  • APET and thick sheet
  • Beverage packaging
  • Custom containers
  • Thick wall containers
  • Bottles
  • Sealing layer for CPET trays
  • Refillable bottles
  • Vendors:
    Available Properties
    • Bulk Density, ASTM D1895, Poured
    • Bulk Density, ASTM D1895, Vibrated
    • Density, ASTM D1505, Film
    • Density, ASTM D1505, Crystalline Density
    • Melt Density, ASTM D1238
    • Viscosity Measurement, EMN-A-AC-G-V-1, Intrinsic
    • Viscosity Measurement, VGAS-A-AN-G-V-1, Pellet, Intrinsic
    • Thickness
    • Film Tensile Strength at Yield, MD, ASTM D882
    • Film Tensile Strength at Yield, TD, ASTM D882
    • Film Elongation at Break, MD, ASTM D882
    • Film Elongation at Break, TD, ASTM D882
    • Film Elongation at Yield, MD, ASTM D882
    • Film Elongation at Yield, TD, ASTM D882
    • Tensile Modulus, ASTM D882, TD
    • Tensile Modulus, ASTM D882, MD
    • Izod Impact, Unnotched (ISO), ISO 180
    • Izod Impact, Unnotched (ISO), ISO 180
    • Tear Strength, Total, ASTM D2582, PPT Tear Resistance, MD
    • Tear Strength, Total, ASTM D2582, PPT Tear Resistance, TD
    • Elmendorf Tear Strength, MD, ASTM D1922
    • Elmendorf Tear Strength, TD, ASTM D1922
    • Dart Drop, ASTM D1709, at -18°C
    • Dart Drop, ASTM D1709, 23°C
    • Film Tensile Strength at Break, MD, ASTM D882
    • Film Tensile Strength at Break, TD, ASTM D882
    • Heat of Fusion, ASTM E793
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Specific Heat Capacity, ASTM E1269
    • Melting Point, ASTM D3418, Crystalline Peak
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 45°
    • Transmission, Visible, ASTM D1003, Regular Transmittance
    • Transmission, Visible, ASTM D1003, Total Transmittance
    • Transmission, Visible, ASTM D1003, Clarity
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.