Excellent cold workability. Fabricated by extrusion, drawing, rolling, impacting, heading, swaging, bending, machining, blanking, roll threading. Applications: electrical connectors, light-duty current-carrying springs, inorganic insulated wire, thermocouple wire, lead wire, resistance welding electrodes for aluminum, heat sinks. Test specimen: wire - 2 mm diameter; 98.5 % cold worked.Inactive per the Copper Development Association. |