MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Nanocyl EPOCYL™ NC R1MY-04 Master Batch Liquid tetrafunctional epoxy Resin for solvent based Formulation Purposes: Dilution Factor 6
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: EPOCYL™ NC R1MY-04 is a Master Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl with a suggested dilution factor of 6. It is specifically developed to enhance the mechanical properties of the final fiber reinforced composite materials. Special features include easy integration and great flexibility in design of new multifunctional materials.

Applications: High performance structural composite parts

  • Automotive (bumpers and other structural parts)
  • Marine, especially sailing boats (structural outer shell in carbon fiber composite, masts and other generic structural parts)
  • Industrial parts (rollers, doctor-blades and wind-mill blades)
  • Sporting equipments (bike frames, hockey sticks, tennis rackets, skis and golf shafts)
  • Aerospace (structural parts and interiors)

Main direct advantages

  • Improved fracture toughness (G1C) of over 100% = higher crack propagation/delamination resistance
  • Improved failure strength: transverse and off-axis (+/- 45°) by over 15% = higher shear resistance
  • Reduced CTE of over 15% = less distorted parts produced
  • No reduction in the Tg = possible to be used in any formulation

Additional advantages in general

  • Electrical properties: induces antistatic properties in the composite parts; excellent for electrostatic painting application
  • Flame resistance: higher resistance to flammability up to UL 94 level on the final fiber reinforced composite
  • Better thermal dissipation: avoids hot-spots during curing, more homogenous temperature

Curing agents EPOCYL™ NC R1MY-04 can be cured or cross-linked with different types of curing agents depending on the properties desired in the final composite like any conventional tetrafunctional based formulations.

IMPORTANT: EPOCYL™ NC R1MY-04 is not an additive in your formulation, it is a substitution product for the equivalent parts of your conventional TGMDA liquid resin. Also, avoid addition of any solvent directly in the EPOCYL™ NC R1MY-04.

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity, Measured with parallel plate in dynamic mode ar 10 rad/s and a strain of 1%.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.