MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting and handling characteristics is required. This dark amber, all liquid formulation contains no solvents, and is easily mixed, handled and applied at room temperature, however a final elevated-temperature cure step is required for complete cure. TRA-BOND 2212 develops strong, tough bonds to metals, glass and glass fabrics, ceramics and many other electronic an aerospace materials. The fully cured adhesive exhibits low weight loss and an improved retention of mechanical properties at elevated service temperatures. It also displays excellent chemical resistance and low permeability to gases and vapors coupled with superior electrical insulation properties. In addition, TRA-BOND 2212 provides very good resistance to water, weather, jet fuels, most petroleum products, salt solutions, mild acids and alkalis, and many other organic and inorganic compounds. For masses over 1/4 gram, step cure the material for 2 hours @ 75°C, followed by 1 hour @ 150°C. This step cure schedule can also be used for low stress applications.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Viscosity, After mixing
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Adhesive Bond Strength, Lap shear, adhesion to glass
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear, Alpha 1
  • CTE, linear, Alpha 2
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time
  • Pot Life, (1 day)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.