MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Premix Thermoplastics PREADD AB 172
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: PREADD AB 172 is a PE-LD based antiblock masterbatch developed for polyethylene films over 35µm in thickness.

The addition of PREADD AB 172 gives following advantages to films:

  • Increased heat conductivity accelerates the cooling of the film. This can lead to capacity increases especially in cases where the natural cooling is insufficient.
  • Antiblocking effect is achieved already at low addition levels.
  • Color change in the extruder takes place faster because of the purging effect.
  • Printability is improved.
  • Heat sealing time and temperature can be lowered.
  • Shrinking time of shrink films can be shortened especially when shrinking is done by infrared radiation. This is a valued advantage e.g. in packaging deep frozen products.

PREADD AB 172 is approved for use in contact with foodstuffs according to FDA and BgVV regulations without limitations.

Information provided by Premix Thermoplastics Inc.

Vendors:
Available Properties
  • Density
  • Additive Loading, CaCO3
  • Maximum Service Temperature, Air
  • Moisture Content, When Produced
  • Shelf Life, Normal Storing Conditions
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Premix Thermoplastics Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.